上一期我们讲了入壳与注液——电芯安了家,电解液也喂饱了极片。但这时候的电芯,还只是一块「半成品」:活性物质沉睡未醒,内部界面也不稳定。把它们唤醒、完成电池的「成人礼」,正是化成(Formation)工序的任务。
Last issue we assembled the cell and filled it with electrolyte. But at this point the cell is still a half-finished product: the active materials are dormant and the internal interfaces are unstable. Waking them up — the coming-of-age ceremony of a battery — is exactly the job of the formation process.
化成不是「测容量」,而是按照预设工艺,对注液后的电芯进行第一次可控充放电,为电池建立一生的工作秩序。化成做得好不好,直接决定电池的寿命、安全与一致性——业内常说,化成决定了电池寿命的上限。
Formation is not capacity testing — it is the first controlled charge-discharge applied to a filled cell, establishing the working order of the battery for life. Whether it is done well decides the lifetime, safety and consistency of the cell. In the industry people say formation sets the upper limit of battery life.
| 01 什么是化成?——第一次充电,命运就此定格 |
化成,简单说就是把注液后的静置电芯拿上化成柜(Formation Cabinet),按设定程序进行首次充放电。它要完成四件事:① 织防护膜——在负极表面生成一层致密的 SEI 膜;② 激活材料——唤醒正负极活性物质,让它们达到最佳性能状态;③ 排出气体——把首次充电产生的气体排掉,防止电池鼓胀;④ 筛选不良——通过化成的电压、内阻数据,把有隐患的电芯提前淘汰。
Formation simply means putting the filled, rested cell on a formation cabinet and running the first charge-discharge cycle. It does four things: 1) build a protective film — a dense SEI layer on the anode; 2) activate the materials — wake up the active materials to their best performance; 3) expel gas — remove gas generated in the first charge to prevent swelling; 4) screen defects — reject risky cells early by monitoring voltage and internal resistance.
理解化成,抓住一个主角就够了——SEI 膜。它是化成的核心产物,也是下一节的主角。
To understand formation, keep one protagonist in mind — the SEI film, the core product of formation and the star of the next section.
| 02 SEI 膜:电池的第一件「防护服」 |

▲ SEI 膜形成原理:锂离子能过、电子不能过(Schematic of SEI film formation)
首次充电时,电解液里的溶剂和锂盐在负极(石墨)表面的低电位环境下发生还原分解,生成一层只有几纳米到几十纳米厚的薄膜——固态电解质界面膜,SEI 膜(Solid Electrolyte Interphase)。它的成分以无机盐(Li₂CO₃、LiF、Li₂O)和有机锂盐为主,化学性质稳定。
During the first charge, electrolyte solvents and lithium salts are reduced on the low-potential anode (graphite) surface, forming an extremely thin film — several nanometres to tens of nanometres thick — called the Solid Electrolyte Interphase (SEI film), composed mainly of inorganic salts (Li₂CO₃, LiF, Li₂O) and organic lithium salts.
这层膜最神奇的地方在于它的选择性:对锂离子导通,对电子绝缘。充放电时,锂离子可以自由穿过它进出负极;而电子和电解液分子却过不去,电解液从此不再被持续消耗。如果这层膜长得不均匀、不致密,电解液就会继续分解、消耗锂源,电池就表现为容量衰减快、内阻偏高、甚至鼓包——所以业内说,化成决定了电池寿命的上限。
The magic of this film is its selectivity: it conducts lithium ions but blocks electrons. Li⁺ can pass freely while electrons and electrolyte molecules cannot, so the electrolyte stops being consumed. If the film is uneven or loose, the electrolyte keeps decomposing — the battery fades fast, its resistance rises, and it may even swell. That is why formation sets the upper limit of battery life.
| 03 化成五步走:一场严谨的「点火仪式」 |

▲ 典型化成流程五步走(Schematic of a typical formation flow)
化成不是插上电源充一次电那么简单,而是一场分阶段、严控参数的电化学「仪式」。典型流程分五步(具体参数以各厂工艺卡为准):
Formation is not a simple single charge; it is a staged, tightly controlled electrochemical "ceremony" of five typical steps (exact parameters follow the plant's process card):
| 化成五步 · Five Steps |
| ① 静置浸润 Rest & Wetting:注液后的电芯先「泡」一会儿。 |
| ② 小电流预充 Preheat / Pre-Charge:用「小火」先慢慢热锅。 |
| ③ 恒流恒压充放电 CC-CV Cycling:主力充放电,SEI 定型。 |
| ④ 排气 / 抽真空 Degassing:把「火气」放出去。 |
| ⑤ 高温老化 High-Temperature Aging:再「焖」一晚上,考验真身。 |
为什么要小电流预充?一句话:SEI 膜的「地基」打得越均匀,后天的循环寿命越长。宁可慢工出细活,也要把第一遍「底漆」刷匀。
Why so small a pre-charge current? A uniform SEI "foundation" means a longer cycle life. Slow and steady wins the race.
| 04 化成设备图鉴:谁在守护这场仪式 |

▲ 负压化成柜、充放电控制单元与高温老化房(Formation equipment overview)
现代锂电工厂的化成分区,通常由三类「主角」撑场:化成柜、负压化成系统、高温老化房——再配合夹具与数据系统协同作业。
A modern formation area normally features three kinds of star players: formation cabinets, vacuum formation systems, and aging rooms — working together with clamping fixtures and data systems.
| 设备图鉴速览 · Equipment at a Glance |
| 化成柜 Formation Cabinet:贯通全线的「大脑」。 |
| 负压化成系统 Vacuum Formation System:边充边「抽气」。 |
| 高温老化房 Aging Room:恒温「焖烧」的考验场。 |
| 夹具 / 加压系统 Clamping System:给电池「压住阵脚」。 |
| 能量回馈单元 Energy Feedback:节能的「充电宝」。 |
| 05 化成方式怎么选?——温度、电流、排气三张牌 |
化成没有「唯一正确解」,不同电芯类型与成本要求会选择不同路线,主要看三张牌:温度、电流曲线和排气方式。
There is no single right answer for formation. Different cell types and cost targets choose different routes along three levers: temperature, current profile, and degassing method.
| 主流路线一览 · Main Routes |
| 按温度:常温化成 vs 高温化成。 |
| 按电流:小电流化成 vs 阶梯 / 脉冲化成。 |
| 按排气:开口化成 vs 负压化成 vs 加盖密封化成。 |
| 按压力:自由化成 vs 约束化成。 |
| 06 质量控制要点:成败都在细节里 |
化成质量好不好,产线上主要盯这几项指标:
Whether formation quality is good or not, the line watches these indicators:
| 关键质量指标 · Key Quality Indicators |
| 首次效率 First-Cycle Efficiency (FCE):SEI 的「学费账单」。 |
| SEI 膜质量 SEI Quality:防护服合不合身。 |
| 内阻 Internal Resistance:界面的「健康体检」。. |
| 温度一致性 Temperature Uniformity:同批电芯要「同温共济」。 |
| 自放电 / 压降 Self-Discharge:静置期的「测谎仪」。 |
再看常见缺陷与对策——套路还是那句:先看现象、再找原因、最后对症下药:
Now the common defects and countermeasures — same drill: observe the phenomenon, find the root cause, then apply the fix.
| 缺陷与对策 · Defects & Countermeasures |
| 首次效率偏低 Low FCE:SEI 吃锂太多。 |
| 内阻偏大 High IR:防护服穿厚了。 |
| 界面黑斑 / 析锂 Black Spot / Li Plating:底漆没刷匀。 |
| 化成后鼓包 Swelling:火气没放干净。 |
| 同批一致性差 Poor Consistency:锅底受热不均。 |
| 07 重点专业词汇双语速查表 |
按主题分组,方便对照记忆——建议收藏慢慢看:
Grouped by theme for easy memorisation — save it for later:
| ① 工序与流程 · Process & Procedure |
| 1化成 Formation |
| 2首次充放电 First Charge-Discharge |
| 3静置浸润 Rest & Wetting |
| 4小电流预充 Pre-Charging |
| 5恒流恒压充电 CC-CV Charging |
| 6高温老化 High-Temperature Aging |
| 7分容 Grading |
| ② 电化学与界面 · Electrochemistry & Interface |
| 1SEI 膜(固态电解质界面膜) Solid Electrolyte Interphase |
| 2负极(负极材料) Anode / Negative Electrode |
| 3电解液 Electrolyte |
| 4首次效率 First-Cycle Efficiency (FCE) |
| 5库仑效率 Coulombic Efficiency (CE) |
| 6析锂 Lithium Plating |
| 7产气 Gas Generation |
| ③ 设备与质控 · Equipment & QC |
| 1化成柜 Formation Cabinet |
| 2负压化成 Vacuum Formation |
| 3真空度 Vacuum Level |
| 4夹具加压 Clamping Pressure |
| 5内阻 Internal Resistance (IR) |
| 6开路电压 Open Circuit Voltage (OCV) |
| 7能量回馈 Energy Feedback |
| 08 学习小贴士:三个一定记住 |
| 三个一定记住 · Three Things to Remember |
| 1. 化成 = 首次充放电 + SEI 膜 + 排气 + 老化。 |
| 2. 小电流预充是为了把 SEI「地基」打匀。 |
| 3. 温度、真空、压力三控,是化成质量的三根支柱。 |
1. Formation = first charge-discharge + SEI film + degassing + aging. 2. Small pre-charge current lays a uniform SEI foundation. 3. Temperature, vacuum and pressure are the three pillars of formation quality.
化成完成的电芯,还要经过容量测定与分级,才能以不同「身价」走上市场——这就是分容(Grading)。下期我们聊「分容与检测:给每一颗电芯『量体裁衣』定身份」,敬请期待!
After formation, the cell still needs capacity testing and sorting to be priced differently on the market — that is grading. Next episode: Grading & Inspection — measuring each cell's capacity and assigning it a grade. Stay tuned!
本系列为「锂离子电池制备(双语教材)」公众号内容,聚焦电池制造各工序的中英文知识。欢迎关注,考试和生产都用得上。
本文为工艺科普性质,文中参数为常见工艺窗口示例,具体以各厂工艺文件为准。This article is for educational purposes; parameters are typical process-window examples and subject to each plant's process documents.